Hi,
I've got a RFQ for 4" Pipes, 10m Long with 4" Fig 602 Thd x Wing Weld Ends and the delivery is within 1 Week.
The question is, Whether, Can i Weld the 6m and 4m Pipes together or it should be 10m single Long pipe?
Since i have the 6m Long pipes already in stock.
Service: H2S.
Please advise. Ofcourse, I can ask the customer, but before that i wanted to be sure.
Your reply is really appreciated.
Thanks & Regards