Dear all,
By referring to the following link of discussion:
I have a situation that a major load bearing support ring for catalyst bed has to be installed to a clad section (CS+316L SS)
The vessel requires PWHT.
Can I strip off the clad where the ring will be located, wled overlay min. of 3/16" thick to the stripped area as a buttered layer, then perform PWHT for the entire vessel. After PWHT, weld the 316LSS support ring to the buttered layer ?
(Our client is asking CS support ring (or clad ring on both sides) directly welded to base metal, and then WOL the entire support ring or stripped area. We are thinking doing other way as mentioned above)
By referring to the following link of discussion:
I have a situation that a major load bearing support ring for catalyst bed has to be installed to a clad section (CS+316L SS)
The vessel requires PWHT.
Can I strip off the clad where the ring will be located, wled overlay min. of 3/16" thick to the stripped area as a buttered layer, then perform PWHT for the entire vessel. After PWHT, weld the 316LSS support ring to the buttered layer ?
(Our client is asking CS support ring (or clad ring on both sides) directly welded to base metal, and then WOL the entire support ring or stripped area. We are thinking doing other way as mentioned above)