I want cut down on the maintenance of my main steam header (50psi) guage line. Right now it is type k copper tubing but it has gotten 2 pin hole leaks in the last year. I was thinking about replacing it with black schedule 40 or maybe 316 SS for longer life? The length of the pipe is about 60 ft. I thought about 316 SS because of less rust and clogging of the gauge and pressure switches at the end of the line. Or should I stick with the copper?