purpletoes
Mechanical
- Sep 1, 2009
- 11
Hello,
I am using a 316SS that is starting to show early signs of corrosion after exposure of 4-6 months. Does anyone have any recommendation for a replacement metal or coating? The metal goes on a water vehicle. The O-ring is also wshowing some MgCl2 and organic Carbon-Oxygen..
Thanks
I am using a 316SS that is starting to show early signs of corrosion after exposure of 4-6 months. Does anyone have any recommendation for a replacement metal or coating? The metal goes on a water vehicle. The O-ring is also wshowing some MgCl2 and organic Carbon-Oxygen..
Thanks