I have a new laserwelded assembly of 304sst tubing. It is for a medical application and oxidation is therefore not a good thing.
The supplier is currently passivating the raw tubes after cutting but before welding.
Is it generally necessary to passivate the final assembly to stabilize the surfaces near the welds? There is no filler material added in welding.
The supplier is currently passivating the raw tubes after cutting but before welding.