I'm considering the use of stainless steel (304/316) in equipment for gas treatment (vessels, heat exchangers and air coolers) due to the presence of CO2 and H2S.
The equipment will be designed in the following pressure/temperature range:
a. 1340 psig/250 F
b. 550 psig/250 F
c. 120 psig/250 F
d. 1350 psig/350 F
Could somebody help me with some guidance in the adequate material selection for this application? (in this case in the material selection for plate, tubes, nozzles)
The equipment will be designed in the following pressure/temperature range:
a. 1340 psig/250 F
b. 550 psig/250 F
c. 120 psig/250 F
d. 1350 psig/350 F
Could somebody help me with some guidance in the adequate material selection for this application? (in this case in the material selection for plate, tubes, nozzles)