Dear all,
Without specifying the minimum carbon content or "H" grade , can plain SA-240-304 SS, which has carbon content from very low up to 0.08% maximum, be used for 536 degC design temperature ? My understanding is only above 540C, high carbon content 0.04% and above is recommended.