Mar 6, 2016 #1 kpm21443 Industrial Joined Dec 20, 2012 Messages 56 Location KW Dear Friends, I have to procure a metal hose with core A182 TP 304 but the manufacturer is offering A182 TP 316. I believe 316 is better than 304. Please advise
Dear Friends, I have to procure a metal hose with core A182 TP 304 but the manufacturer is offering A182 TP 316. I believe 316 is better than 304. Please advise
Mar 6, 2016 1 #2 mrfailure Materials Joined Aug 7, 2011 Messages 817 Location US 316 has added molybdenum. It is more corrosion resistant and generally is considered an upgrade. Upvote 0 Downvote
Mar 6, 2016 1 #3 EdStainless Materials Joined May 20, 2004 Messages 16,374 Location Waukesha WI USA And the mechanical properties are very similar. Unless you are using 304 for some very specific reason the swap to 316 should work fine. = = = = = = = = = = = = = = = = = = = = P.E. Metallurgy, Plymouth Tube Upvote 0 Downvote
And the mechanical properties are very similar. Unless you are using 304 for some very specific reason the swap to 316 should work fine. = = = = = = = = = = = = = = = = = = = = P.E. Metallurgy, Plymouth Tube