We have a 302 SS compression spring that rides inside a borosilicate glass (Pyrex) tube. The wire dia is about .025 and the spring force is nominally 1 lb.
After about 250,000 cycles of the spring, it appears the spring is rusting on the OD where it rubs on the glass. The environment is room temp, 4 psia air, in an "office-like" setting. There are many rust colored particles nearby.
The spring was not passivated after coiling.
Any ideas on how this could be happening? Could the rubbing remove the protective layer on the SS?
Nearby there is a steel part that is not protected from corrosion and there is no rust on that part.
Thanks,
Tom
After about 250,000 cycles of the spring, it appears the spring is rusting on the OD where it rubs on the glass. The environment is room temp, 4 psia air, in an "office-like" setting. There are many rust colored particles nearby.
The spring was not passivated after coiling.
Any ideas on how this could be happening? Could the rubbing remove the protective layer on the SS?
Nearby there is a steel part that is not protected from corrosion and there is no rust on that part.
Thanks,
Tom