From Your photos, the seal looks like it is made from either (a) sintered/compacted iron/graphite/copper mix; or (b) is a pure sintered/compacted graphite material... and was intended for high temp service.

It would pay to have the material analyzed by a lab. There might be a material standard IF the material can be verified.

As far as a industry standard for the shape and material... I doubt it. HOWEVER... The following specs MIGHT actually provide a clue after-all.

SAE AIR1077 Metallic Seal Rings for High Temperature Reciprocating Hydraulic Service

MIL-M-24130 and /1, /2 and /3 METALLIC SEAL RINGS, NON-INTEGRAL GENERAL SPECIFICATION FOR [spec is distribution controlled by Navy]

NOTE.
All metallic seals/gaskets I found were hollow and crushed/distorted on installation.

Regards, Wil Taylor

o Trust - But Verify!
o We believe to be true what we prefer to be true. [Unknown]
o For those who believe, no proof is required; for those who cannot believe, no proof is possible. [variation,Stuart Chase]
o Unfortunately, in science what You 'believe' is irrelevant. ["Orion", Homebuiltairplanes.com forum]
 
If you bypass the dialog box and simply copy the link and paste that directly into your thread, you can reference as many files as you want.

TTFN (ta ta for now)
I can do absolutely anything. I'm an expert! faq731-376 forum1529
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor

Back
Top