Hi all,
we are in the process to derate the 30" API 5L B dia oil pipeline (158km), wall thickness is 80% gone due corrosion and this line was installed some 40 years back.
as per barlow's equation MAWP is coming 112 psi,my question is, can i further derate the line as operation manager requested to derate untill line is composite repaired.I don't have copy of B31.4 for reference.
thanks
10815L
we are in the process to derate the 30" API 5L B dia oil pipeline (158km), wall thickness is 80% gone due corrosion and this line was installed some 40 years back.
as per barlow's equation MAWP is coming 112 psi,my question is, can i further derate the line as operation manager requested to derate untill line is composite repaired.I don't have copy of B31.4 for reference.
thanks
10815L