Hello all -

Have a short question, I am trying to find out how many threads per inch a 3/4" diameter A36 anchor bolt would have. Any information on where I might be able to obtain this information would be appreciated.

Thanks
 
Standard coarse screw thread is 3/4-10. I cannot believe that they would deviate from a coarse thread pitch.
 
The AISC Manual provides this information for standard bolts.
 