and if the service temperature is between -40 and 600F you could use a 25 Cr duplex such as 2507 or 255 or Xeron 100.
You can also add N08925 to the above list. Every major stainless producer makes at least one 6% Mo grade.
make the part by press forming a piece of plate into a cylinder, weld with matching filler, solution anneal (2175-2200F), water quench, and pickle.
= = = = = = = = = = = = = = = = = = = =
Plymouth Tube