Jul 28, 2005 #1 nettwork Mechanical Joined Jul 28, 2005 Messages 1 Location US Looking for any specs to assist in machining 2519T87 Aluminum. Feeds and speeds for pocket milling would be helpful. Thank you
Looking for any specs to assist in machining 2519T87 Aluminum. Feeds and speeds for pocket milling would be helpful. Thank you
Jul 28, 2005 1 #2 metengr Materials Joined Oct 2, 2003 Messages 15,478 Location US bGood luck trying to find free information regarding this aluminum armor material. Here is a start for your search; http://www.alfed.org.uk/templates/alfed/reports_search.asp?PageId=121 http://www.stormingmedia.us/reports/metallurgy-and-metallography-132.html Upvote 0 Downvote