I am in the process of contacting several Tank Manufacturing companies to provide Carbon Steel Tanks for our Wastewater Treatment Plant. The caustic is 25% with the maximum temperature leaving the Chemical Plant being 165 F. I have seen that with temperatures reaching 165 F, stress relieving welds may be necessary. My questions are, should the tank have stress relief welds? Also, would the tank need to have an internal lining to prevent any type of corrosion? Any information on this will be greatly appreciated.