Good day,
I need to place 23lbs zinc anodes on a barge. I'm going withe the convention
Total surface area of anodes = 1% of wetted surface.
Now that gives me the total surface area of anodes, 57sq ft, but how do i adequately space these anodes? is there a convention for this or a rule of thumb or something I can refer too?
Thank You
Justin