A supplier is offering SA-790 S31803 (2205) pipe "with no heat treat (HT-0)". This is for Sec VIII, Div 1 use.
SA-790 requires all pipe to be furnished in heat-treated condition.
If using this pipe, the fabricator will be responsible for final heat treat and resulting mechanical properties, no?
Regards,
Mike
SA-790 requires all pipe to be furnished in heat-treated condition.
If using this pipe, the fabricator will be responsible for final heat treat and resulting mechanical properties, no?