Looking for static and fatigue properties for 21-6-9 SS.

Thanks,

jetmaker
 
Replies continue below

Recommended for you

In what mechanical strength condition?

= = = = = = = = = = = = = = = = = = = =
Still trying to help you stop corrosion.
formerly Trent Tube, now Plymouth Tube
eblessman@plymouth.com
or edstainless@earthlink.net
 
Looking for Tube.

Thanks,

jetmaker
 
The tubing that is used for hydrol tubing is cold drawn to elevated strength. The spec is AMS 5561 and the UTS is 142-162 ksi.
Is this the material that you are looking for?

= = = = = = = = = = = = = = = = = = = =
Still trying to help you stop corrosion.
formerly Trent Tube, now Plymouth Tube