I am redesigning a small vessel for use in Europe at -20F (-29C). Currently it is made of SA53B,E shell, SA414G heads, SA36 machined nozzles. My understanding is that these materials cannot be rated -29C in Europe without impact testing. But I understand that I can achieve -29C if I switch to SA524 shell, SA516-70 (normalized) heads, and SA516-70 (normalized) machined fittings AND FOLLOW THE FOLLOWING STEPS:
1) Limit carbon content to .23%, Phosphorous to .035%, Sulfur to .025%
2) Employ Fig UCS-66 to show -55F at 20J impact
3) Adjust to 27J using API579
I would appreciate hearing comments on how sensible this plan is, and if there are better material choices than I gave.
1) Limit carbon content to .23%, Phosphorous to .035%, Sulfur to .025%
2) Employ Fig UCS-66 to show -55F at 20J impact
3) Adjust to 27J using API579
I would appreciate hearing comments on how sensible this plan is, and if there are better material choices than I gave.