metman

Materials
Feb 18, 2002
1,187
1. Do we need to get the specification from Global
Engineerig or is it avilable on the web?

2. Any ideas on a supplier for Initial Outside Diameter of
3.75 inch X Wall thickness .375-.5 inch?

3. I first went to FAQ's but not much help also tried
Google > Online metals etc.

Thanks in adance.

Leonard

Jesus is THE life,
Leonard
 
Replies continue below

Recommended for you

Leonard,

First, I could not find on the government standard website ( You will need to order SAE AMS 4086 either from Global or from SAE.

Second, the following distributors supply 2024-T3 Al tubing that meets SAE AMS 4086:




I am not sure who manufactures this tubing. I tried Alcoa, but they only seem to do 6xxx series as standard. Kaiser probably makes this out of the Chandler, AZ facility.
 