Does anyone know why 100% ultrasonic inspection is mandated for e-beam welds?
 
Replies continue below

Recommended for you

Too high a probability for Lack-of-Fusion with the EB process. UT-shearwave is the best method for detecting and quantitfying L.F.
 
That's an interesting observation. Do you have any literature you can point me too, that backs that up? I read that UT is best suited for detecting planar flaws, while x-ray and UT are equally suitable for detecting volumetric flaws (see below).
I suppose the thinking is that, you could also have planar flaws. Thus, UT is sensible because it could pick up flaws that X-ray couldn't.
It seems though that 100% inspection is overkill in certain cases based on part dimensions and weld characteristics.


For reference, the paper with the comparison between x-ray and UT is:

Jack Spanner, “Effectiveness of Substituting Ultrasonic
Testing for Radiographic Testing for Repair/Replacement”
ASME Conf. Proc. 2005, 33 (2005)
 
edit: I see that lack of fusion is considered a planar flaw which supports using UT.
 
Concur on "100% UT not needed". This is an automated process. Those tend to be either All Good, or All Bad. Sampling of segements that are carefully chosen will work.
 