Galambos
Structural
- Jun 27, 2005
- 231
I have small room (15'x12') that requires a 2" concrete topping over a newly placed slab on grade with a vapor barrier.
I am going to use sikacrete 211 as my topping, without a bonding agent, so as to not trap moisture between the barrier and the bottom of my topping.
i am concerned about cracking, and if i use the 24 x thickness rule for unreinforced concrete, my 1" deep sawcut joints would be spaced at 48" o.c. Does this seem reasonable for this application? Am i missing something? Would it be best to use fibers?
I am going to use sikacrete 211 as my topping, without a bonding agent, so as to not trap moisture between the barrier and the bottom of my topping.
i am concerned about cracking, and if i use the 24 x thickness rule for unreinforced concrete, my 1" deep sawcut joints would be spaced at 48" o.c. Does this seem reasonable for this application? Am i missing something? Would it be best to use fibers?