While reviewing some records at work on some reactors in our Hydrogen unit that they may not have been Stress Relieved to the proper temperature.
The material is SA-387 Gr.11 Class 2 (1-1/4% Cr) which is a P-4 Material. Our records indicate that the vessels were stress relieved at 1100 deg F. The current code calls for a minimum temperature of 1200 deg F.
We are having trouble finding a copy of the 1980 code with the 1982 Addenda to reference to determine whether this was the acceptable temperature at the time of construction. The earliest we have been able to check is the 1989 edition. Any help in shedding some light on this would be greatly appreciated.
The material is SA-387 Gr.11 Class 2 (1-1/4% Cr) which is a P-4 Material. Our records indicate that the vessels were stress relieved at 1100 deg F. The current code calls for a minimum temperature of 1200 deg F.
We are having trouble finding a copy of the 1980 code with the 1982 Addenda to reference to determine whether this was the acceptable temperature at the time of construction. The earliest we have been able to check is the 1989 edition. Any help in shedding some light on this would be greatly appreciated.