1971 ASME Section VIII, Div. 1
SA240TP 316 Plate at 200 and 300 F - both high(@ both temps 18.7) and low values please (@200 18.7, @300 16.1)
SA240TP 316L Plate at 200 and 300 F - both high(@200 and 300 -15.6) and low values please(@200-13.2, @300-11.8)
It is not listed under TP, that is referred to as Tube or pipe product form. The plate is listed as
316L, and 316.
There was a note to the higher values Summarized:
Higher values where developed at temps where you may get slight deformation, and are not
recommended on flange faces ( exceed 62.5% , but not 90% yield)