I have a code vessel built in 1955.
Material SA-285-C. What was the temperature break for the allowable stress. Was it 650F?
 
Replies continue below

Recommended for you

Yes. For most of carbon steel, the code listed only one allowable stress for -20F thru 650F.
 
The temperature break is for time dependent properties above 650 deg F.
 
So it would have been built to the 1952 edition of Section VIII which lists 13,750 psi as the basic allowable stress in tension for SA285-C up to 650°F.

jt
 