1
- #1
I have an application that is currently using Half Hard 304. This grade is not stiff enough for my application and I'd like to use 17-7PH to get a stiffer part.
The application uses very thin sheet (0.2mm to 0.7mm thick) that is formed then laser welded together.
My questions are:
(1) Is 17-7PH available in thin sheet in this range?
(2) I have read that 17-7PH when transformed to condition C at the mill is magnetic. It there a heat treatment process that does not result in a magnetic part?
The application uses very thin sheet (0.2mm to 0.7mm thick) that is formed then laser welded together.
My questions are:
(1) Is 17-7PH available in thin sheet in this range?
(2) I have read that 17-7PH when transformed to condition C at the mill is magnetic. It there a heat treatment process that does not result in a magnetic part?