The data I have for 17-7ph ch900 has a yield strength of 231 KSI and ultimate of 239 KSI.
An engineer designed a small leaf spring with this material that in tests plastically deforms (stretches).
This has to be impossible, right? With the yield and tensile right on top of each other, this is a very brittle material, correct? Maybe the parts we have were not heat treated properly to the ch900 spec.
Sanity check - if you're designing a spring, you shouldn't intend to stress it beyond the yield point, especially with a brittle material, correct?