Jan 21, 2011 #1 cezarcbc Industrial Joined Jan 19, 2011 Messages 4 Location BR The material 17-4PH has an equivalence to any ASTM material?
Jan 21, 2011 #2 metengr Materials Joined Oct 2, 2003 Messages 15,478 Location US Go to this web site and look at product forms http://www.aksteel.com/pdf/markets_products/stainless/precipitation/17-4_PH_Data_Sheet.pdf Upvote 0 Downvote
Go to this web site and look at product forms http://www.aksteel.com/pdf/markets_products/stainless/precipitation/17-4_PH_Data_Sheet.pdf
Jan 24, 2011 #3 valvit Mechanical Joined Jan 25, 2007 Messages 60 Location US ASTM A564 Grade 630 Upvote 0 Downvote
Jan 26, 2011 #4 EdStainless Materials Joined May 20, 2004 Messages 16,351 Location Waukesha WI USA in some specs they use the UNS S17400 = = = = = = = = = = = = = = = = = = = = Plymouth Tube Upvote 0 Downvote