17-4-PH trim material

Status
Not open for further replies.

arash807

Mechanical
Aug 8, 2012
48
Can we use SS410 instead of 17-4-PH in a control valve which is installed in steam service?
 
Replies continue below

Recommended for you

Yes this is a globe valve with follow conditions:
inlet pressure=40 barg
operating temperature=410 centigrade
plug material:F6NM+stellite
cage material:17-4-PH
we are going to replace the cage with ss410.is it possible or not?
 
While 410 stainless steel has the strength component - it lacks the corrosion resistance properties of 17-4 PH.
17-4 PH would be preferrable over 410 stainless steel.
 
add more to "valveexpert":
you should choose 17-4PH HT1150 hardened cage, which is good for high temperature (410 C deg) erosion-corrosion resistance, and also higher strength at high temperature. the seat ring should be solid cobalt/stellite hardened,if you can make the cage seat surface hardened with alloy6, it would be better. this is a super-heated steam application, the steam can cut the metal quickly if it leaks or operating at low flow condition. 410SST is not very good for this severe process.


Get help and return with helps!!.
 