Now I see HH1150 or H1150+1150 from BearCraft. Apparently this is two times through H1150 process heat treat. BearCraft publishes a separate set of mechanicals that go with it. Also now I am seeing published mechanical properties for Condition A solution annealed state, where before Carpenter and others refused to publish condition A mechanicals. Also see that ductility for condition A can be all over the map. How about the material community bringing some order to this chaos?
For years I advised my shop not to use 17-4 at condition A for load bearing because of unpublished mechanicals. Now I am having second thoughts. What is the consensus of this august body?