We will be doing some NDE LPI inspections on some Furnace tubes 16Cr-11Ni-2.5MoCb. We don't expect any repair but just in case we want to make sure we are covered with a WPS. As for code the client states Examination shall be required per ASME B31.3. With regards to the material, it looks to be P8 material. But it doesn't seem common like 16Cr-12Ni-2Mo. I'm not sure what the abbreviation (Cb) is as well at the end. Can anyone tell me typically what P number this is or how to find that out? Or what welding rod is typically used for this?

Thank you.
 
Replies continue below

Recommended for you

You’ll have to look in ASME section II, part A for that specific material and see if there is an associated P-number with it.

Cb is the old designation for Columbium, now known as Niobium (Nb).

The devil is in the details; she also wears prada.
 