bdruehl
Civil/Environmental
- Oct 27, 2004
- 92
possible for bid job..
16 foot cantilever deck with main beams 13 foot spacing (13 ft trib to the cantilevered 7x20 glulam beams which extend into the residence say 15 feet)...100 lb live load required!!! haha!
the glulams are rotted. NO POSTS allowed ofcourse by request by owner. idea is to cut the beam at the exterior of house then the fun begins with the attachment to the non cantilvered portion of the glulams (which are exposed) with some steel member scabs. i have my doubts to the ability of exiting glulams (and their attachments too) which probably were designed to half or less of the 100 lb balcony live load required now.
thoughts, or even better, anyone do this so i dont recreate the wheel and make a square?
16 foot cantilever deck with main beams 13 foot spacing (13 ft trib to the cantilevered 7x20 glulam beams which extend into the residence say 15 feet)...100 lb live load required!!! haha!
the glulams are rotted. NO POSTS allowed ofcourse by request by owner. idea is to cut the beam at the exterior of house then the fun begins with the attachment to the non cantilvered portion of the glulams (which are exposed) with some steel member scabs. i have my doubts to the ability of exiting glulams (and their attachments too) which probably were designed to half or less of the 100 lb balcony live load required now.
thoughts, or even better, anyone do this so i dont recreate the wheel and make a square?