Is anyone using 15-5 stainless as a spring?
Since 17-7 is tough to get, I was wondering if anyone has had success & if they have a hardening and tempering process
to get the material to RC44-51. The spring is low deflection
(.015") max and is flat.
Thanks for any help.
Since 17-7 is tough to get, I was wondering if anyone has had success & if they have a hardening and tempering process
to get the material to RC44-51. The spring is low deflection
(.015") max and is flat.