My Customer material requirement was 15-5 PH per AMS 5759. An additional requirement was to heat treat to condition H1025 per AMS 2759.
I purchased material from the Mill as Cond 1025H but was not certified to AMS2759 for the heat treat. The Mill says that his Condition H1025 is for unfinished bar and that final Heat Treat to condition H1025 per AMS 2759/3 should be accomplished by us since we are manufacturing a completed machined part. I'm confused, My customer says they will not accept the parts.
I purchased material from the Mill as Cond 1025H but was not certified to AMS2759 for the heat treat. The Mill says that his Condition H1025 is for unfinished bar and that final Heat Treat to condition H1025 per AMS 2759/3 should be accomplished by us since we are manufacturing a completed machined part. I'm confused, My customer says they will not accept the parts.