I'm looking for the inherent minimum bend tolerence for 14 G steel. Is there a good book/soure where this can be found?

Cheers!

Joe
 
Replies continue below

Recommended for you

Ehhh there is no inherent min bend for 14Gauge.... You'll have to figure out which temper youve got and what quality. Then from teh rockwell B value and a good steel hand book you cna get the minimum bend radi for perpendicular and parallel bends.

nick
 
The rule of thumb for low carbon steel is 1 x thickness is the minimum bend radius. There are special cases though. Reducing the carbon to .05-.10 improves the bendability and bending across the grain will allow smaller bend radius. These assumptions are for air bending where the die opening width is 8 times the material thickness. If the die opening is greater than 8T than the radius on the part will not match the punch and will not be a smooth radius.

In practice unless you are willing to spend additional money for non-standard bending tooling you will be bending 14ga with a 1/16" radius punch and utilize a 5/8" vee die. You could probably use a 1/32" radius punch however the part will come out with a distorted (non-radius) bend and the punch will have excessive wear.
 