The guyed towers I have looked at fell in a similar kinked manner due to the falling mast being constrained by the guys. Although there was secondary buckling in the tower mast, the initial cause was excessive slack in the guys or the loss of a guy, resulting in the mast exceeding slenderness and deflection limits.