557835
Materials
- Dec 17, 2009
- 2
hi. we want to cast 1.4742 steel with a coreless induction furnace. but we have a problem because of this material 1.4742. 1.4742 material has 0,7-1,0 aluminium and 0,12 carbon, 18 chrom. so its difficult that cast this material. we casted but the casting is too bad; it has surface cracks and too many slags on the face. I think its reason Aluminium.( % 1 ) So, what can we do?
- using filter?
- changing gating system?
- using maybe some stabilizator elements for aluminium?
or what? please help me..
- using filter?
- changing gating system?
- using maybe some stabilizator elements for aluminium?
or what? please help me..