Jul 7, 2005 #1 ktm2003 Mechanical Joined Jun 6, 2005 Messages 2 Location IS Hello all, can anybody tell me the difference between the material 1.0619 and 1.7365. Thank you in advance.
Hello all, can anybody tell me the difference between the material 1.0619 and 1.7365. Thank you in advance.
Jul 10, 2005 1 #2 Goahead Aerospace Joined Jul 13, 2003 Messages 625 Location IL Hello, WS 1.619 also known as GS-C25 Weight % C=0.18-0.23 Si=0.60 Mn=0.50-1.20 P=0.03 S=0.02 equivalent to ASTM A216 Gr. WCC WS 1.7365 also known as GX15CrMo5 Weight % C=0.25-0.30 Si=0.15-0.25 Mn=0.60-0.80 P+S=0.035 max Cr=3.00-3.30 Mo=0.45-0.55 http://www.welding-advisers.com/ Upvote 0 Downvote
Hello, WS 1.619 also known as GS-C25 Weight % C=0.18-0.23 Si=0.60 Mn=0.50-1.20 P=0.03 S=0.02 equivalent to ASTM A216 Gr. WCC WS 1.7365 also known as GX15CrMo5 Weight % C=0.25-0.30 Si=0.15-0.25 Mn=0.60-0.80 P+S=0.035 max Cr=3.00-3.30 Mo=0.45-0.55 http://www.welding-advisers.com/
Jul 18, 2005 Thread starter #3 ktm2003 Mechanical Joined Jun 6, 2005 Messages 2 Location IS Thank you for this Upvote 0 Downvote