Ch-ch-ch-changes.

Would you interpret the dimensions given in UW-21 as minimums with the maximums shown in appendix 2 for a loose-type arrangement? This appears to have been a hurried change when compared to the completeness in the '08 Addenda...and this interpretation seems consistent between the two addendas.

--------------------------------
Fitter, happier, more productive
 
weld is lesser 1/4" or thickness of nozzle. I think most use the nozzle thickness as many users don't like an unwelded corner and inside appendix 2 uses full pipe thickness

they are not addressing the standard 1/8" between toe of weld and the corner of raised face. but appendix 2 says max is 1/4" + wall of pipe.

we standardly use pipe wall + 1/8 for set back with a pipe wall + 1/4" max set back

Now that being said, we never weld a slip on flange in pressure situation, just internal non-pressure.

 
So what do you interpret to be the meaning of "tmin" in the note under the figure? t(required) of the neck? tr + CA?

Agree with BigTank, this looks a little hasty.

Regards,

Mike
 
My mistake, probably tmin per UG-16?
 
I believe 1.4tmin is meant to be 1.4tn as is required in B31.1-2004

Where tn is the nozzle or pipe wall thickness

Also worth noting another inconsistency in B31.3-2004 T overscore is used in the rule for xmin.

At any rate something for ASME to fix/clarify in the next edition or addenda of section VIII.
 
All,

Yes, this is an error which did not get caught prior to final printing.

The new weld dimension requirements in UW-21 were extracted from B31.1 and should mirror them in the upcoming Errata.

In the meantime, BradLancour is correct:

1.4tmin should read 1.4tn.

Xmin = 1.4tn or thickness of hub, whichever is smaller.

tn= nominal pipe wall thickness.