In stainless steels, specially austenitic, problem of sesitization occurs if we cool slowly in the range of 400 to 700C. Therefore quenching of aust. SS is done commonly from higher temps. In sensitization, Cr combines with Iron which precipitates on the grain boundaries & can cause corrosion &...