  1. iowaguy

    Bright dipping extruded aluminum part

    I am bright dipping an extruded aluminum part. ( size about 4 inches X 4 inches) The reason for bright dipping is to get a high apperance shine. MY QUESTION IS: Will the bright dip process provide a coating that will give me a rust prevention characteristic? How long will this last to...
  2. iowaguy

    Bright dipping extruded aluminum part

    I am bright dipping an extruded aluminum part ( size about 4 inches X 4 inches ) The reason for bright dipping is to get a high appearance shine. MY QUESTION IS: Will the bright dip process provide a coating that will give me a rust prevention characteristic? How long will this last to...
  3. iowaguy

    extruded aluminum that will accept ground

    I am interested in making a extruded aluminum part. The aluminum is 6063-T6. The part must accept a ground. Would making the extrution non-anodized make my part capable of being grounded? When the part is anodized I cannot get a ground. Please suggestions?
  4. iowaguy

    weldable rust proof coatings

    I need to bring across the ocean parts of 8 guage carbon steel wire (rust is a concern). I need a cost effective rust proof coating that also has weldability once the parts reach the US. Thanks