I have a batch of partially used pickling acid (sulfuric acid) which mistakenly had some flux introduced into it.
The ferrous concentration is about 4% currently.
The flux is a mixture of ammonium chloride, potassium chloride, zinc chloride, and sodium chloride.
Is there a process to remove via...