  1. managingdirector

    UV cure silicone rubber

    Hello everybody, Who knows more about UV cure silicone rubber, here is the link: www.medicaldesignbriefs.com/component/content/article/1105-mdb/features/10454http://files.engineering.com/getfile.aspx?folder=a70acb2a-f807-4718-a5b5-3bb3e86d67bb&file=0711_mdb_feat1_fig_01.png
  2. managingdirector

    How to improve silicone rubber parts compression set?

    Thank you very much Stancom,Fumed silica is effective tensile strength,high voltage resistance, hardness and more transparency in silicone rubber.but because of the total cost there is limitation in use.
  3. managingdirector

    How to improve silicone rubber parts compression set?

    Dear Johnnymat, thank you very much, heavy loaded is for high voltage resistance. so,please let me know either ATH or MgO is more suitable to achieve both high voltage and compression set?
  4. managingdirector

    How to improve silicone rubber parts compression set?

    Dear Stancom Thank you very much for your helpful guidance, our formulation is for extrusion as bellow items: 1-Silicone gum rubber-----------150.00k 2-precipitate silica------------105.00k 3-Hydroxyl oil(silicone oil)------6.50k 4-Stearic acid -------------------0.60k 5-Aerosil 200(fumed...
  5. managingdirector

    How to improve silicone rubber parts compression set?

    Dear friends kindly let me know how can I improve silicone rubber parts compression set?.
  6. managingdirector

    EPDM profiles-hot air cure

    Thank you very much for your comment,I would explain more that now we are producing silicone rubber profiles, actually I wanted to know that, is it possible we shift from silicone compound to EPDM compound for the same profiles? if yes then is it needs we design a special formula or any changing...
  7. managingdirector

    EPDM profiles-hot air cure

    Dear Graham, it's 8meters per minute.
  8. managingdirector

    EPDM profiles-hot air cure

    It's highly appreciate to somebody tell me, how can I cure EPDM profiles in hot air tunnel?, the temp.is 300C and tunnel length is 12M and extruding out put is 45 grs./min. thanks in advance.
  9. managingdirector

    cure EPDM profiles in hot air tunnel.

    Dear racookpe1978 and 3DDAVE I would appreciate both of you for your kind attentions,I mentioned the technical information,and also I will try to find the EPDM rubber chemical component supplier but still looking for to know totally is it possible to cure EPDM in hot air tunnel?,then if yes how...
  10. managingdirector

    cure EPDM profiles in hot air tunnel.

    Dear friend Thanks a lot for your kind attention,The temperature is 300C and the curing time is 1minute,and the tunnel length is 12meters, material out put is 450grs per minute.hope the information would be useful.
  11. managingdirector

    cure EPDM profiles in hot air tunnel.

    It's highly appreciate to somebody tell me, how can I cure EPDM profiles in hot air tunnel?