  1. m3brunof

    Overlay WPS?

    Are you guys following QW-453 Corrosion-Resistant Overlay or Hard-Facing Overlay?
  2. m3brunof

    Overlay WPS?

    Can I develop an overlay WPS using QW-451.1? For instance it would be a GMAW P1 to P1 or P8 to P8. Is this possible without actually welding up a groove?
  3. m3brunof

    Boretech WPS and WOPQ

    I will be qualifying new WPS for P1, P8 and P6gr4. I will be using GMAW with short circuit transfer. Since these WPS will be used for weld build up only, should I follow QW-453 corrosion-resistant overlay or QW-453 hard-facing overlay?
  4. m3brunof

    Boretech WPS and WOPQ

    I know the welder operator needs to be qualified per QW-484B, but can I take a WPS that was qualified manually and use it with the Boretech welder? Or does it need its own WPS?
  5. m3brunof

    Boretech WPS and WOPQ

    In my situation, the Boretech will be used for weld repair and weld build up only. The welding performed will be like an overlay weld. How should I set up the weld test, if the welding performed will be like an overlay?
  6. m3brunof

    Boretech WPS and WOPQ

    I will be using the GMAW process, the thickness will range from 1/8" to 2". The welding will be performed on pump impellers mostly. I hope this info helps.
  7. m3brunof

    Boretech WPS and WOPQ

    Hey guys, I will be qualifying a new WPS and WOPQ using a Boretech welder. So far I've done only plate WPS, and am a little unfamiliar with pipe and automated equipment. What is the best size diameter and thickness combo to qualify a WPS and WOPQ simultaneously with a Boretech? This will be done...
  8. m3brunof

    ASME WPS with cast iron

    I'm actually reviewing a customers WPS from Asia, the welding was done with SMAW
  9. m3brunof

    ASME WPS with cast iron

    Can you qualify a WPS with a cast iron ie; A439 per ASME section IX? A WPS per ASME requires side bend tests which I don't think would pass. What are my options on qualifying this type of material?
  10. m3brunof

    ASME base metal welding?

    If my WPS is qualified for 3/16" to 8" base metal thickness, can I do a repair weld on a base metal that's 14" thick? As long as I stay within the 8" limit? Or do I need a different WPS which would have 14" within the range?
  11. m3brunof

    How many Charpy V specimens?

    If I qualify two processes together on plate, GMAW for root and FCAW for filler, will two test plates be enough for Tensile Test, Bend Test and Toughness Test? Thanks for any help
  12. m3brunof

    ASME vs MIL-STD 248

    What are the main differences between these two standards?
  13. m3brunof

    How many Charpy V specimens?

    I'm using ER80S-D2 and E81T1-Ni1. So do I need 3 total tests, or 3 tests for HAZ, 3 for weld metal, 3 for base plate?
  14. m3brunof

    How many Charpy V specimens?

    I searched the forums but could not find an answer. I'm qualifying a WPS with GMAW and FCAW on 1-1/2" P1 gr2 plate. GMAW root and FCAW filler and cover passes. Charpy testing will be at -50 F. This will be done per B31.3. From what I've read, it looks like I will need 3 specimens per set of...
  15. m3brunof

    Anyone familiar with the ACCP/NDE Program?

    Is anyone familiar with the ACCP/NDE Program?