INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Looking for book(s) on aluminum extrusion process

Looking for book(s) on aluminum extrusion process

Looking for book(s) on aluminum extrusion process

(OP)
Good Morning,
I'm just starting the extrusion learning process.
I'm looking for reference materials, books, on the Aluminum Extrusion Process.
I've found one from ASM titled Aluminum Extrusion Technology.
Are there any others out there.
Looking for basic information on the process, what affects it , the tooling , design and tooling tolerances, etc.
Thanks for your information.
Hinged.

RE: Looking for book(s) on aluminum extrusion process

ALCOA produced and published some very good books working with Aluminum and had a very good one on extrusions.  You might try the old book stores as I think they are out of print.   

RE: Looking for book(s) on aluminum extrusion process

I have a basic design manual for aluminum extrusions published by the company I work for that we send out to customers on occasion.  I have some of the more informative sections in pdf format so they are e-mailable.  If you are interested, e-mail me at joules1971@yahoo.com.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members! Already a Member? Login



News


Close Box

Join Eng-Tips® Today!

Join your peers on the Internet's largest technical engineering professional community.
It's easy to join and it's free.

Here's Why Members Love Eng-Tips Forums:

Register now while it's still free!

Already a member? Close this window and log in.

Join Us             Close