First of all, hi everyone, im new here,

second, i've been going crazy trying to find the electrical resistivity of galvanized steel(zinc-coated) and i haven't found anything, i have found however the resistivity of steel and stainless stell, but i don't know what effect the zinc does to its resistivity, so im asking if anyone knows where can i find this info? any knows? help please?
 
Replies continue below

Recommended for you

Why do you need it?
If you know the thickness of Zn, you can calkulate as 2 Zn
and 1 Fe layers of known thickness if they are chemically
pure -- if not, you may have to measure it.



<nbucska@pcperipherals.com>
 
ah thanks, i needed it for an rf simulation program, that material wasn't there but i found it in it's a source for material info, but thanks a lot anyway
 