Kindly advice on below,

P355QH1(Un assigned group as per ASME IX)where as P355NH assigned group as per ASME IX?
BOTH HAVE SAME CHEMICAL AND MECHANICAL PROPERTIES.
 
Replies continue below

Recommended for you

Cannot replace an assigned material with an unassigned one.

DHURJATI SEN
Kolkata, India


 
QH is quenched and tempered weras NH is normalised
 