True stress and strains for Steel + ductility

Status
Not open for further replies.

Daemon1

Student
Mar 15, 2022
20
Hello, I wish to model a steel connection in Abaqus with steel S275 but I don't have the corresponding parameters :
-yield stress / plastic strain (I'd like up have the table of values of possible)
- damages parameters such as :Failure stress, stress triaxility

Please can some one send me these values or indicate to me where I can find it 🙏🏾, thanks in advance
 
Replies continue below

Recommended for you

I only can help you with the fact that the yield strength is usually in the range of 275 to 390 MPa, and the typical plastic deformation in tension is in the range of 0.2 to 0.25.Bye.
 