INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Contact US

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

The manufacterer of the stripper ov

The manufacterer of the stripper ov

The manufacterer of the stripper ov

(OP)
The manufacterer of the stripper overhead accumulator has choosen the material of shell and head astm a- 387 gr22 cladding with monel although a-387 is good at elevated pressure and temperature . I don't know what the reason of using cladding for monel.

RE: The manufacterer of the stripper ov

Monel would prevent corrosion due to condensation, which is basically acidic corrosion.

DHURJATI SEN
Kolkata, India


RE: The manufacterer of the stripper ov

Cladding is a way to get the high corrosion resistance at a lower cost

--- Best regards, Morten Andersen

RE: The manufacterer of the stripper ov

You are welcome,..... ENGRANIA

MJCronin
Sr. Process Engineer

RE: The manufacterer of the stripper ov

@ENGRANIA
"stripper overhead accumulator" - what does this stripper strip and what does this accumulator accumulate?

RE: The manufacterer of the stripper ov

(OP)
@ MJCronin
Thank you...

RE: The manufacterer of the stripper ov

Engrantia

Monel cladding is for corrosion purposes, but in what service will be aplicated the stripper overhead vessel?

regards

luis

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members! Already a Member? Login



News


Close Box

Join Eng-Tips® Today!

Join your peers on the Internet's largest technical engineering professional community.
It's easy to join and it's free.

Here's Why Members Love Eng-Tips Forums:

Register now while it's still free!

Already a member? Close this window and log in.

Join Us             Close