We need to glue awning canvas (100% acrylic) on wood and we don’t know how, we are looking for an alternative to contact glue given that applying the adhesive to both of the materials is not feasible in this case due to their shape.

We’ve tried white glue but it does not adhere strong enough. A symmilar but stronger glue would be perfect.

Cyanocrilate is strong but the area to bond is too big.

Any idea?
Thanks

 